T215M5
M Machine Forming Tap
Material ID: 7174125
Thread forming tap with chamfer form C with a 2-3xP plug lead, for ISO-Metric thread M5 with 0.80 mm pitch and 6HX class of fit, dimensions according to DIN 2174 standard with 6.0mm shank and 4.9mm square drive, solid carbide with TiCN coating for 3xD through or blind hole threading in steel and cast steel, ferritic, martensitic and austenitic stainless steel and wrought or cast aluminium and copper or copper alloys
Product Feature
Product Detail
Description | Value |
---|---|
Product name | T215M5 |
Product number (SAP) | 86031145 |
EAN number | 7320760704646 |
Thread diameter size (TDZ) | 5 |
Thread pitch - millimeter (TP) | 0.8 mm |
Overall length - millimeter (OAL) | 70 mm |
Overall length - inch (OAL) | 2.7559 inch |
Threading length - millimeter (THL) | 16 mm |
Threading length - inch (THL) | 0.6299 inch |
Connection diameter - inch (DCON MS) | 0.2362 inch |
Connection diameter - millimeter (DCON MS) | 6 mm |
Flute count (NOF) | 5 |
Clamping width - inch (WSC) | 0.1929 inch |
Clamping width - millimeter (WSC) | 4.9 mm |
Clamping Length - inch (LCS) | 0.315 inch |
Clamping Length - millimeter (LSC) | 8 mm |
Premachined hole diameter - inch (PHD) | 0.1811 inch |
Premachined hole diameter - millimeter (PHD) | 4.6 mm |
Gross weight - grams | 30.38 |
ISO | T215M5 |
Ordering code ANSI | T215M5 |
Cutting Conditions
Suitability | vc | f | |
---|---|---|---|
P1.1 - Free machining sulfurized carbon steel with a hardness of < 240HB | Primary use | 60 m/min | |
P1.2 - Free machining sulfurized and phosphorized carbon steel with a hardness of < 180HB | Primary use | 68 m/min | |
P1.3 - Free machining sulfurized/phosphorized and leaded carbon steel with a hardness of < 180HB | Primary use | 68 m/min |
Suitability | vc | f | |
---|---|---|---|
P2.1 - Plain low carbon steel containing < 0.25%C with a hardness of < 180HB | Primary use | 68 m/min | |
P2.2 - Plain medium carbon steel containing < 0.55%C with a hardness of < 240HB | Primary use | 60 m/min | |
P2.3 - Plain high carbon steel containing > 0.55%C, with a hardness of < 300HB | Primary use | 45 m/min |
Suitability | vc | f | |
---|---|---|---|
P3.1 - Alloy steel with a hardness of < 180HB | Primary use | 44 m/min | |
P3.2 - Alloy steel with a hardness of 180 - 260HB | Primary use | 36 m/min | |
P3.3 - Alloy steel with a hardness of 260 - 360HB | Primary use | 30 m/min |
Suitability | vc | f | |
---|---|---|---|
P4.1 - Tool steel with a hardness of < 26HRC | Primary use | 26 m/min | |
P4.2 - Tool steel with a hardness of 26 - 39RC | Primary use | 22 m/min |
Suitability | vc | f | |
---|---|---|---|
M1.1 - Stainless steel, ferritic with a hardness of < 160HB | Primary use | 34 m/min | |
M1.2 - Stainless steel, ferritic with a hardness of 160 - 220HB | Primary use | 29 m/min |
Suitability | vc | f | |
---|---|---|---|
M2.1 - Stainless steel, martensitic with a hardness of < 200HB | Primary use | 31 m/min | |
M2.2 - Stainless steel, martensitic with a hardness of 200 - 280HB | Primary use | 25 m/min | |
M2.3 - Stainless steel, martensitic with a hardness of 280 - 380HB | Possible use | 21 m/min |
Suitability | vc | f | |
---|---|---|---|
M3.1 - Stainless steel, austenitic with a hardness of < 200HB | Primary use | 29 m/min | |
M3.2 - Stainless steel, austenitic with a hardness of 200 - 260HB | Primary use | 25 m/min | |
M3.3 - Stainless steel, austenitic with a hardness of 260 - 300HB | Primary use | 23 m/min |
Suitability | vc | f | |
---|---|---|---|
M4.1 - Stainless steel, austenitic-ferritic or super-austenitic with a hardness of < 300HB | Primary use | 25 m/min | |
M4.2 - Stainless steel, precipitation hardening austenitic with a hardness of 300 - 380HB | Possible use | 22 m/min |
Suitability | vc | f | |
---|---|---|---|
N1.1 - Pure aluminium and wrought aluminium alloys with a hardness of < 60HB | Primary use | 70 m/min | |
N1.2 - Wrought aluminium alloys with a hardness of 60 - 100HB | Primary use | 53 m/min | |
N1.3 - Wrought aluminium alloys with a hardness of 100 - 150HB | Primary use | 35 m/min |
Suitability | vc | f | |
---|---|---|---|
N2.1 - Cast aluminium alloys with a hardness of < 75HB | Primary use | 98 m/min | |
N2.2 - Cast aluminium alloys with a hardness of 75 - 90HB | Primary use | 98 m/min | |
N2.3 - Cast aluminium alloys with a hardness of 90 < 140HB | Primary use | 80 m/min |
Suitability | vc | f | |
---|---|---|---|
N3.1 - Free-cutting copper-alloys materials with excellent machining properties | Primary use | 50 m/min | |
N3.2 - Short-chip copper-alloys with good to moderate machining properties | Possible use | 50 m/min | |
N3.3 - Electrolytic copper and long-chip copper-alloys with moderate to poor machining properties | Primary use | 38 m/min |