S2603.0
End Mill
Ordering number: 6706913
Short series end mill with 4 flutes, diameter 3mm with 9mm length of cut and 57mm overall length, according to DORMER standard with a 6mm plain shank, solid carbide with AlCrN coating, 40° helix with differential pitch and 4° rake angle for shoulder milling and plunging in martensitic, austenitic and super-austenitic, Duplex or precipitation hardening stainless steel, high-temperature alloys, chilled, hardened cast-iron and hardened steel <55HRC
Product Feature
Product Operation
Product Detail
Description | Value |
---|---|
EAN number | 7320760684627 |
EDP number | 46706913 |
Product name | S2603.0 |
Ordering code ANSI | S2603.0 |
Gross weight - grams | 24.9 |
Cutting diameter - millimeter (DC) | 3 mm |
Connection diameter - millimeter (DCON MS) | 6 mm |
Depth of cut maximum - millimeter (APMX) | 9 mm |
Overall length - millimeter (OAL) | 57 mm |
Flute count (NOF) | 4 |
Radial rake angle (GAMF) | 4 |
With Neck | Yes |
ANSI | S2603.0 |
ISO | S2603.0 |
Cutting Conditions
Suitability | vc | f | |
---|---|---|---|
P4.3 - Tool steel with a hardness of 39 - 45HRC | Primary use | 318 ft/min | 0.0006 inch/rev |
Suitability | vc | f | |
---|---|---|---|
M2.3 - Stainless steel, martensitic with a hardness of 280 - 380HB | Primary use | 318 ft/min | 0.0006 inch/rev |
Suitability | vc | f | |
---|---|---|---|
M3.3 - Stainless steel, austenitic with a hardness of 260 - 300HB | Primary use | 325 ft/min | 0.0005 inch/rev |
Suitability | vc | f | |
---|---|---|---|
M4.1 - Stainless steel, austenitic-ferritic or super-austenitic with a hardness of < 300HB | Primary use | 318 ft/min | 0.0005 inch/rev |
M4.2 - Stainless steel, precipitation hardening austenitic with a hardness of 300 - 380HB | Primary use | 272 ft/min | 0.0005 inch/rev |
Suitability | vc | f | |
---|---|---|---|
S1.3 - Titanium alloys, a hardness of 280 - 360HB | Primary use | 230 ft/min | 0.0005 inch/rev |
Suitability | vc | f | |
---|---|---|---|
S2.2 - High-temperature Fe-based alloys with a hardness of 200-280HB | Primary use | 184 ft/min | 0.0005 inch/rev |
Suitability | vc | f | |
---|---|---|---|
S3.2 - High-temperature Ni-based alloys with a hardness of 280 - 360HB | Primary use | 131 ft/min | 0.0005 inch/rev |
Suitability | vc | f | |
---|---|---|---|
S4.2 - High-temperature Co-based alloys with a hardness of 240 - 320HB | Primary use | 105 ft/min | 0.0005 inch/rev |
Suitability | vc | f | |
---|---|---|---|
H1.1 - Chilled cast iron with a hardness of <440HB | Primary use | 587 ft/min | 0.0004 inch/rev |
Suitability | vc | f | |
---|---|---|---|
H2.1 - Hardened cast iron with a hardness <55HRC | Primary use | 348 ft/min | 0.0003 inch/rev |
Suitability | vc | f | |
---|---|---|---|
H3.1 - Hardened steel with a hardness of <51HRC | Primary use | 387 ft/min | 0.0003 inch/rev |
H3.2 - Hardened steel with a hardness of 51 - 55HRC | Primary use | 318 ft/min | 0.0003 inch/rev |